RE: [MW:10204] Can I use E 7018 in Pipe root runs? What's the disadvantages?

Good morning all
 
As per Mr. Goswami. Please find attached latest tech guide from Bohler on Pipe electrodes.
 
Regards,
 
Garry Hunt
Bhhler Welding Group Canada
 

From: pgoswami@quickclic.net
To: materials-welding@googlegroups.com
Subject: RE: [MW:10147] Can I use E 7018 in Pipe root runs? What's the disadvantages?
Date: Sat, 5 Mar 2011 00:50:08 -0500

Mr. Srinivasan

E-7018 is universally accepted low hydrogen electrode, helping many welding engineer and welders to produce quality welds. However for pipeline welding , especially for root passes, this electrode has some limitations. In our electric utility we do not perform a lot of cross country pipeline welding. But there're some such pipelines for  carrying natural gases, to fire in the boilers.Field welding  and desired quality of such piping's may not be easy always.
There're some practical welding issues with E-7018 for root passes, e.g less digging arc, which may cause inconsistent root penetration, greater slag volume  and less friable slag, which is  sometimes difficult to move. Generally our experiences is with E-7010 root +E-7018 filling passes.
The attached product of Bohler looks promising. Feel free to dig up more information and I'm sure some members from BTW would be more than happy to help you further in your queries.
Thanks.

Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of James, GeraldJayakumar
Sent: Wednesday, March 02, 2011 4:33 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:10104] Can I use E 7018 in Pipe root runs? Wats the disadvantages?

I suppose it requires highly skilled welders to get uniform root penetration which could pass Radiography testing. For Piping it is normal practice to use GTAW for the Root Run & Next pass, & for remaining passes joint can be completed using SMAW E7018

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Engineer Mech
Sent: Wednesday, March 02, 2011 2:22 PM
To: Materials & Welding
Subject: [MW:10087] Can I use E 7018 in Pipe root runs? Wats the disadvantages?

Hi All,

Can I use E 7018 in Pipe root runs? Wats the disadvantages?
Can i go E 7018 root run& filler WPS qualification?

Regards
Srinivasan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchanged in this group are members personnel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

**********************************************************************
Confidentiality Notice

This communication and the information it contains:-
(a) Is intended for the person(s) or organization(s) named above and for no other person(s) or organization(s). 
(b) May be confidential, legally privileged and protected in law. Unauthorized use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postmaster@fwuk.fwc.com.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchanged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...