Re: [MW:35628] Can we avoid PWHT for P No.5A to P No.1 , 10mm weld joint ?

Dear Sir, 

It is a condensate receiver tank and it is a design requirement from client side.

Regards, 
Saravanan. 
S.KOREA 

On Thu, 22 May 2025, 9:26 pm Raghuram Bathula, <raghurambathula@gmail.com> wrote:
Why do you use P22 nozzles on CS?

On Thu, 22 May 2025, 16:24 PARAI Reaction Channel, <saravanshyla@gmail.com> wrote:

Dear Sirs ,

 

We have a project with both shell and Reinforcement Pad materials SA516-70, 10 mm Thk ( P No.1 ) and the Nozzle is SA335-P22, 4" Sch 120 , 

11.1 mm ( P No.5A ) Thk.

 We already have a qualified WPS & PQR with 8mm GTAW and tested about 10 years ago by other welding engineer, for P No,.5A to P No.1 without PWHT and it was satisfactorily passed and we 

have used that WPS & PQR for the previous project 10 years ago and no 

issues found without PWHT.

 Now for the new project, we are going to use the same WPS and apply 

Preheat ( 204 to 250 Deg C ) as per the WPS for 10mm Shell Thk by 

multipass welding, refer to the below sketches.





So, i would like to confirm whether PWHT is mandatory as per UCS-56-4 ?

Can we avoid PWHT for this 10mm weld joint ?


Or Should we do buttering with ERNiCr-3 on P No.5A bevel and butt weld 

with same filler for this dissimilar joint to avoid PWHT after making new 

PQR with buttering?


Please confirm soon.


Thanks and Regards,

Saravanan Sornam,

ANSAN-Si,

S.Korea 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALV1rk%2Biby3LDhuASFD6Sx3wD6mhOVKRXA8dsJCQcfO-yNsjhQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3DgSEPtoFpp%2BtcafrEOrNOzUxFt_9E4TfiPwfyP21JHdg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALV1rkJt_cnVR3wJkwRy%3DHUD9Qviu-HO7EmcYVbQQmmkV2v8iA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...