Skip to main content

Re: [MW:35562] SS FILLER

I suppose Mr. Viswas is looking for the process details. Normally these materials are used in Refinery & Petrochemical plants.

1. If it is a Pressure equipment check in the design data sheet.
2. If it is a piping, then get the piping class from ISO dwg and refer in Piping material specification for the process fluid such as nitric acid etc..

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Thursday 24 April, 2025 at 06:03:51 pm IST, Elavarasan Mech <elavarasan1861994@gmail.com> wrote:


Our project SA182 F44 ,S31254 

ELA


On Wed, 23 Apr 2025 at 7:53 PM Akhilesh Kumar <akhileshlikes@gmail.com> wrote:
Greeting to All of you! 

Could you please confirm if the P-No.-8  Group1 material (ASTM A316L) WPS can use for P.-No.-8 Group4 material (ASTM A312) 

Please confirm or required due to group. 

Thank You! 
With Regards, 


On Wednesday, April 23, 2025, Elavarasan Mech <elavarasan1861994@gmail.com> wrote:
Dear All 
 Please clarify below 

we have qualified WPS( P No 8 GR 1 To P NO 8 GR 1). Filler metal Er 316l ( Fno:6)
 
In our current project UNS S31254 ( PNO 8 Gr No 4)
We useing a filler wire ER2594 (Fno 6 )


Can we use above wps for this project with filler metal ER2594  Please guide me 
CODE ASME SEC IX 





regards 
ELAVARASAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ymviaYs8wTi0ZC2v_L9PsxT9%3DRsHdQNgCDbJJSZsjdyug%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAE1xz0Mu6EWvE1jSmrYNfwTSKq027-b3rn_QJ3jynQKuVezSfQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ymM3PQqoOFhA8Y_xmfYax2b-8uMdx%3DPFCUonufW-Je8Dw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...