Hi

The code we use is AWS D1.1

On Thu, 22 May 2025 at 08:19, Venkatachari Muralidharan <ennappan@gmail.com> wrote:
Hi

To my knowledge 
If you are qualified as welding coordinating personal under ISO 14731 namely International welding engineer / technologist / specialist then you can carry out  the questions 1 to 4 as mentioned in your email and for which code of construction to fabricate and weld the component and certify welders . 

The WPS / PQR / WPQR you need to follow the formats form of the code you design and follow for fabrication and welding pl 

Muralidharan V
22/05/2025
ENNAPPAN  CONSULTANTS
HUMAN  RESOURCES , SKILLS  , TALENTS AND SPOTTER

WELDING    EDUCATION ,  TRAINING & ENGINEERING 

E.M.NUMBER – 33 - 001 - 21 - 50170 - PART II 

CELL - + 91  99624 56967  

EMAIL -

ennappan@gmail.com

venkatacharimuralidharan@gmail.com



On Thu, 22 May 2025 at 07:31, Rene Alvarado <rene.alvarado.lozano@gmail.com> wrote:

Please check Standard ANSI / ASME N45.2.6 Qualifications of Inspection, Examination, and Testing Personnel for Nuclear Power Plants

 

René Alvarado


El vie, 16 may 2025 a la(s) 6:57 a.m., Desmond Meyer (meyerdesmond87@gmail.com) escribió:

Dear Experts,

I hope this email finds you well. I'm reaching out for advice on a current project where we're performing flux core welding. We need to qualify our welders and ensure compliance with relevant standards.

As a QC Level 1, I'm wondering if I'm qualified to:

1. Evaluate and qualify welders?
2. Write Procedure Qualification Records (PQR)?
3. Develop Welding Procedure Specifications (WPS)?
4. Conduct Welder Qualification Tests (WQT)?

Specifically, we're working with flux core welding, and I'd appreciate guidance on the requirements and best practices for welder qualification and documentation.

Could you please provide advice or point me in the direction of relevant resources?

Thank you for your expertise and assistance.

Best regards,

DESMOND 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKM3ENkVYsu3ge4sr_WQQC1RU_8%3DN6%2B54eUU1umt_p%3DJvQWnoA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHbC_j1VcaS3R4gRJDUJaC3whjq3Kf0H3CS1UH_v8LozWC3dqg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CABc%2BPwUoH3j1%3De0YxfmLYnHaxj50yRNiEWioa4mQr1%2B%2BZURucQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKM3ENm6492Q_4k%2Bt%2BCC1JHMcYQBRtWRa-HVijQaOK-BtJNPSA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...