Re: [MW:35590] Clarification on WPS Applicability for SS316L to Duplex Welding per ASME Section IX

P10 H to P8 
ASME sec IX 
WPS is acceptable
If API582 or other Client specifications are applicable , then revisit the decision.
Review Discuss with QA ,Welding proceed accordingly 
Sent from my iPhone

On 1 May 2025, at 11:32 PM, Deerendra Karanth <dkaranths@gmail.com> wrote:



If supplementary requirements for impact testing are applicable, a change in A-number will require new WPS qualification; however, if impact testing is not required, the existing WPS can be used as long as the P-Number and F-Number remain unchanged.

BR, 

Deerendra.. 



On Thu, 1 May, 2025, 18:57 Nambirajan Avudaiappan, <nambirajanavudaiappan@gmail.com> wrote:
Dear ranijith,
My question regarding the applicability of WPS only.

On Thu, 1 May 2025 at 14:03, Ranjit singh <ranjit450@gmail.com> wrote:
Dear sir,

We are facing problem in welding crack for desimilar metal like en19 hub dia 350mm thick 200mm and shaft en19 dia 140mm groove weld 28mm.

Process:- SMAW
Pre heating 200-250 degree.
Observation:- crack 

Regards,

Ranjit
9216671043

On Thu, May 1, 2025, 1:40 PM Nambirajan Avudaiappan <nambirajanavudaiappan@gmail.com> wrote:

Dear Experts,

I hope this message finds you well.

I would like to seek your clarification regarding the applicability of an existing WPS.

We have successfully qualified a WPS for welding SS316L to Super Duplex using ER2594 filler metal. Both base materials are classified under P-No. 8 to 10H, and the filler metal falls under F-No. 6.

However, our actual production requirement involves welding SS316L to Duplex Stainless Steel using ER2209, which also falls under F-No. 6, and the base metals remain under P-No. 8 to 10H.

As per ASME Section IX, since the base metal P-Numbers and filler metal F-Numbers remain unchanged, could you please confirm whether the existing WPS is valid for this application as well, or if a new qualification is required?

Thank you in advance for your guidance and support.

Regards,

Nambirajan A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2XnCz1x1PWFoGvwdFQQCG-e_8K_ksgtNPtt2mwocbS4Gw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BE2JLO6r4aNeUGLsCJdcKXpwF9ju6wthJoEpub5-PSiZ6fovQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2UjQfSLHGNbtSCDYfzsxxoD_sQ84Jqih_CO5xa1Xxu3Sg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG0nF9Fv%2B8%3DAGFvJ05Ajkccw42bVAQDc9J72x63gy9XHnGmBcg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...