Wednesday, June 7, 2023

[MW:34266] Provide suitable welding electrode for Alloy steel .

Dear Quality Team,

 

Pl provide suitable electrodes  for as attached PMI composition.

 

I was selected for the E11018 electrode.  With Preheat 150 deg.

 

What is your option.., and welding procedure ?

 

Equipment : Air receiver Header ,Size Dia 250mm X 4mm.

Application : ESP / Bag filter pulsing header.

Services : 12 years old, power plant .

Defect:  Fillet weld center of portion crack observed.  

Chinese Power Plant.  

 

 


 

 

--
Kind Regards

Sunthar A
+91 9894100888

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKWjHyMzv1pn7SzcfPKc12nPViZ9qvRwVSPgxfQurU1w64MyTA%40mail.gmail.com.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...