Re: [MW:34255] Max allowable machining thickness for qualifying PQR

You can do machining as per your requirement But for qualification range your governing thickness will be 12.6mm. 

On Mon, May 29, 2023, 8:04 AM JITHIN GOPINATH <2k9jithin@gmail.com> wrote:
Sir,
Can anyone advice me about the maximum allowable machining thickness for qualifying PQR.
For example I have a pipe with thickness 15.88 I want to reduce the thickness to 12.6 is that possible? If there any limitations for machining the thickness..
Please advise...

Regards
Jithin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAT3KQ7iuBvsLQTWYfFSvHRunVEd%2B_jHsd_vEZMVKozOt%2BKcfw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA7RJJOztM8LG%3DLSWYARaiCXd2v4tQRDEptnWTECUdJvQtRHdg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...