Re: [MW:34236] Dissimilar chemical composition weld

Hi,

1. Alloys are acceplable if the alloying elements are each within 10% of the specifled range of values. 


2. Welds with consumables that match, or nearly match, the base meal composilion shall be within +12.5% of the ranges allowed in ASME SEC IIC for each element.Chemical Composition of Material specs must be verifled/avallable.

thank you 


On Tue, 23 May 2023 at 6:57 AM Sintha Aidroos <iti.sintha@gmail.com> wrote:
Dear experts,
                Please advise about weld metal deposit  composition for base metal cuni 90/10 (UNS C 70600) and filler wire CuNi70/30 (UNS C 71500) combination of this material.We checked PMI at weld joint area but composition is not matching with ASME sec II part C .Can you give guidance for any PMI acceptance criteria?Here I attached PMI report for your review.

As per ASME sec II filler metal nickel percentage is 29-32 % and copper remaining.


 Regards

Aidroos      

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM11Z9UL_Wt3U7Rzr06B1XsBxQwmXYeSDsUp6seDEc1%3DOmNAfg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAERXeW%3DD%3Dj7Ub%3D61BtMzSP2HJW7U4oORz9vcnusWk8pvhcxmTg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...