 Hi, 
Check  with kobelco  they have some TG-X series filler wire without purging that may be used for Rootpass.
Thanks and Regards, 

On Mon, May 22, 2023, 6:10 AM Anand Elankumaran <email2uranand@gmail.com> wrote:
Dear experts,

Could you please check and advise the below query.

  • Whether the back purging is a quality requirement or the ASME code is insisting on back purging on SS material while doing the GTAW process.
  • Whether we can qualify SS -GTAW PQR without back purging or the ASME code does not allow doing PQR for austenitic steels without a back purge?
  • Kindly advise how to do it without purging in SS GTAW Welding . Planning for PQR as well 


--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChxEbF6gP%2BwCFusuTWnJpmbZMst%2BM1qCz3y2fHr0mRaY1Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPFTRWnof0A4VYJ2KqAUppcX-z2fKCrmoFL70DOHyxqEYRv6mQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...