As you know, Low hydrogen Electrods shall be baked (350 degree for 2 hours), but in this case the workshop supervisor didn't bake them, instead of that, he kept them directly in holding oven.
So shall these electrods scrapped or baked and used?
On Mon, May 22, 2023, 7:47 AM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
The question is not clear--Pl elaborate the querySent from my iPhoneOn 22-May-2023, at 8:40 AM, Mahmood Al-Hinai <hyna4444@gmail.com> wrote:Dear all experts,--If Low Hydrogen Electrods kept directly in a holding oven without backing, and later on it was observed, so how to rectify?Shall be scraped or backed?
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEuX%2Bd%3D-LvqWgQ-qVC0KqtfcVEP8_haQFEHEK%2BqSw87Ss8ms%3Dg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F033F967-E354-40A3-A48C-628EBF34D5E9%40gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEuX%2BdkYTotNmVDfoL%2B9m8Sm%3DtdS17yE2%2BjShedgM1LWDJG-0Q%40mail.gmail.com.
Comments