Re: [MW:34220] Parent material Thickness For GTAW process

pl correct the following--- ASME SEC IX is not a Construction code, it is Reference code.
Since ur base metal thickness is 11mm, Qualification range for GTAW of Base metal is 5mm to 22mm

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, May 22, 2023 at 8:40 AM Prasad rao <prasadrao31@gmail.com> wrote:

Dear All,


We have prequalified WPS of combination  GTAW+SMAW

 

Qualified material :4"  Dai X Sch-120(11.02mm)

Garde : ASTM A106 GR B

Welding Process :  GTAW +SMAW


Construction Code : ASME SEC IX

 

Root/ Hot : ER70S-6 Dai 2.4

Fill 1,2 ,3 : E7018 Dai 3.2

Cap           : E7018 Dai 2.5.

 

With Above WPS I would like to extract new WPS for GTAW Process. Please Kindly confirm  what shall be the range  for GTAW process  for parent material thickness . Kindly advice. with reasoning.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEML-XTU9igHwEckWNCH4r_XuWwozo4qRoC_yEXuMvkQrpSuEg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMBc8CmU4LyyMA8mjrJB9CZDv0ieOtbx_%2BT2GX7jXTrRw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...