Re: [MW:34217] Low Hydrogen Electrods

The question is not clear 
Pl elaborate the query

Sent from my iPhone

On 22-May-2023, at 8:40 AM, Mahmood Al-Hinai <hyna4444@gmail.com> wrote:


Dear all experts,

If Low Hydrogen Electrods kept directly in a holding oven without backing, and later on it was observed, so how to rectify?
Shall be scraped or backed?


--