Monday, May 8, 2023

Re: [MW:34203] Impact Testing requirements for PQR

Please provide below details

1. MDMT (minimum Design Metal Temperature)
2. Involved Material Grades like ASTM A105 / 106 Gr.B / 333 Gr.6  etc..
3. Applicable design code Like ASME B 31.3
4. Material thicknesses

Thanks & Regards

J.Gerald Jayakumar




On Monday, 8 May, 2023 at 06:49:53 pm IST, Jackson Raj <jacksonraj007@gmail.com> wrote:


Dear all

Is it mandatory to do Impact Testing in PQR our clients doesn't approaching to us to do Impact Testing they only required impact Testing in Forging Material Tee and flanges.

That's why we are doing Impact Testing in PQR.

Thanks & Regards
Jack

On Fri, May 5, 2023, 6:18 AM Srinivas Rao <srinivas.nitt11@gmail.com> wrote:

in addition to above one may consider PWHT requirements if anything applicable as per the design and client spec, if PWHT applicable one may consider additional PQR's or based on the construction code exemption recommendations PQR's Can be avoided by following pre-heat requirements of the construction code.

Regards, 
Srinivas Rao
On Thursday, May 4, 2023 at 3:22:12 PM UTC+4 james gerald wrote:
Appreciate efforts and initiative from ENG.Ahmed.

Just to share. 2 PQR's 6mm & 23mm is sufficient.

There is an ASME Interpretation stating PQR qualified on 6mm and higher thickness qualifies in the range from 16mm.  Someone please share the Interpretation.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 4 May, 2023 at 03:45:32 pm IST, 'Ahmed Osman' via Materials & Welding <material...@googlegroups.com> wrote:


3 PQR's may be sufficient , 6mm (3-12) 10mm (10-20) 23mm (16-46) 

Best Regards ,
ENG. Ahmed Osman



On Wednesday, May 3, 2023 at 08:44:46 a.m. GMT+3, Jackson Raj <jackso...@gmail.com> wrote:


Dear all,

In Our project has 3 inch to 24 inch and it's thickness 5.49mm to 45.24mm and Impact Testing required for above thickness.
Please clarify how many PQR are required for this job 
Please consider the Impact Testing also mentioned each PQR thickness qualify 

Regards
JJ

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALgFOaXAKmJFBKLz39ZoUn%3Dnwi4Er11Qts17%2BbWyQkBOYML4Eg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/95dfb447-8b39-4c0b-a898-6f5683be32ecn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALgFOaV79Dt0jr5nNzR1f75utkFDJ6U2mh7rSjS52R9o_ko_Cw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...