Re: [MW:34192] Impact Testing requirements for PQR

ASME B31.3 2018 has the requirements for specimen Thickness BM requirements as per below Snap shot.


Inline image
But in ASME B31.3 BM Thickness requirement for Impact is revised. See below snap shot.

Inline image


Inline image



Thanks & Regards

J.Gerald Jayakumar




On Thursday, 4 May, 2023 at 04:52:07 pm IST, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Appreciate efforts and initiative from ENG.Ahmed.

Just to share. 2 PQR's 6mm & 23mm is sufficient.

There is an ASME Interpretation stating PQR qualified on 6mm and higher thickness qualifies in the range from 16mm.  Someone please share the Interpretation.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 4 May, 2023 at 03:45:32 pm IST, 'Ahmed Osman' via Materials & Welding <materials-welding@googlegroups.com> wrote:


3 PQR's may be sufficient , 6mm (3-12) 10mm (10-20) 23mm (16-46) 

Best Regards ,
ENG. Ahmed Osman



On Wednesday, May 3, 2023 at 08:44:46 a.m. GMT+3, Jackson Raj <jacksonraj007@gmail.com> wrote:


Dear all,

In Our project has 3 inch to 24 inch and it's thickness 5.49mm to 45.24mm and Impact Testing required for above thickness.
Please clarify how many PQR are required for this job 
Please consider the Impact Testing also mentioned each PQR thickness qualify 

Regards
JJ

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALgFOaXAKmJFBKLz39ZoUn%3Dnwi4Er11Qts17%2BbWyQkBOYML4Eg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/895749842.194908.1683193821769%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1060130634.2136276.1683196250168%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...