Re: [MW:34186] Impact Testing requirements for PQR

3 PQR required as per your job thickness.

On Wed, 3 May 2023, 11:14 AM Jackson Raj <jacksonraj007@gmail.com> wrote:
Dear all,

In Our project has 3 inch to 24 inch and it's thickness 5.49mm to 45.24mm and Impact Testing required for above thickness.
Please clarify how many PQR are required for this job 
Please consider the Impact Testing also mentioned each PQR thickness qualify 

Regards
JJ

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALgFOaXAKmJFBKLz39ZoUn%3Dnwi4Er11Qts17%2BbWyQkBOYML4Eg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-ipzX-1iY%2BVRY8Y66nz1Yh44mere%3DAA36VoAuXXrEGeqA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...