[MW:34252] RE: 34251] Re: PQR WITH TWO WELDING PROCESS TO SEPERATE IT

Yes its possible, You can go for only SMAW considering all other essential variable

 

QW-200.2(f) One WPS. Several WPSs may be prepared from the data on a single PQR (e.g., a 1G plate PQR may support WPSs for the F, V, H, and O positions on plate or pipe within all other essential variables). A single WPS may cover several sets of essential variable ranges as long as a supporting PQR exists for each essential and, when required, supplementary essential variable [e.g., a single WPS may cover a thickness range from 1/16 in. (1.5 mm) through 11/4 in. (32 mm) if PQRs exist for both the 1/16 in. (1.5 mm) through 3/16 in. (5 mm) and 3/16 in. (5 mm) through 11/4 in. (32 mm) thickness ranges].

 

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of biennd
Sent: Wednesday, May 31, 2023 12:15 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:34251] Re: PQR WITH TWO WELDING PROCESS TO SEPERATE IT

 

Hi there,

 

May you check in which standard refers to.

I understood, ASME IX allowed for thickness of test coupon more than 13 mm.

 

Thanks

Bien ND

 

On Tuesday, May 30, 2023 at 6:28:48 PM UTC+7 QA/QC wrote:

Dear master 

 

please can you advise me i have some doubt 

in our project i have a PQR qualify with gtaw + smaw butt weld 

Detail :

 

7.14 to 20 (CS & LTCS)
GTAW  5 mm +SMAW 9
ER70S-6 + E7018-1 

 

and i want to qualify to only SMAW PROCESS is it possible or no 

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8e67b12e-4012-4530-91ce-7940fb52f5d6n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...