Wednesday, May 31, 2023

[MW:34251] Re: PQR WITH TWO WELDING PROCESS TO SEPERATE IT

Hi there,

May you check in which standard refers to.
I understood, ASME IX allowed for thickness of test coupon more than 13 mm.

Thanks
Bien ND

On Tuesday, May 30, 2023 at 6:28:48 PM UTC+7 QA/QC wrote:
Dear master 

please can you advise me i have some doubt 
in our project i have a PQR qualify with gtaw + smaw butt weld 
Detail :
 
7.14 to 20 (CS & LTCS)
GTAW  5 mm +SMAW 9

ER70S-6 + E7018-1 


and i want to qualify to only SMAW PROCESS is it possible or no 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8e67b12e-4012-4530-91ce-7940fb52f5d6n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...