[MW:34231] Re: Minimum distance between two circumferential pipe joints

Check consruction code and client specification for minimum diatances between welds , each will have a different recommentdations . refer and follow 
Example : ASME B 31.3 - does not given any recommendations on this subject.

Regards,
Srinivas Rao
Welding Engineer 
On Monday, May 22, 2023 at 12:52:04 PM UTC+4 Parminder Singh wrote:
minimum 4t 

On Monday, May 22, 2023 at 1:19:50 PM UTC+5:30 port dickson wrote:
Dear Experts,

                              We need your advice regarding minimum distance requirements between 2 circumferential pipe joints .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7c45aba5-0f4c-4acd-b84a-92f0449a1ef6n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...