Dear all, Client has reduced the MDMT as -45Deg.C from -60Deg.C. In this case can we use E7018-1 to weld materials  SA 537 Class1, SA 333 Grade 6, SA350 Gr.LF2 (Changed from LF3) and SA 420 WPL9.

Also suggest me the suitable electrode to weld these materials with SS304 & SS16.

looking forward your replies.

On Friday, 28 April 2023 at 08:28:49 UTC+5:30 amso...@gmail.com wrote:
  Dear Experts,

Please suggest us the suitable electrode to weld the SA 537 Class1, SA 333 Grade 6, SA350 Gr.LF3 and SA 420 WPL9 with the Impact temperature at -60 Deg.C

Also Shell Thickness of SA 537 Class1 is 12mm & 16mm. Hence is this vessel required PWHT

I have chosen below electrode to weld these materials.

E8018-C3
ER80S-Ni1

E81T5-Ni3C

E81T5-Ni2C

Requesting expert opinions in these regards

Thanks and Regards,

MS


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/69db8d89-6ce3-4a99-897a-e93aa2e0e165n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...