Saturday, October 29, 2022

Re: [MW:33642] Re: PWHT requirement _ASME B31.8

Material

Pipe : API 5L X60
Hub : A694 Gr.F60

On Sat, Oct 29, 2022 at 12:04 PM Mohd Siraj <mohd52100@gmail.com> wrote:
whats material?

On Tuesday, October 25, 2022 at 6:51:03 AM UTC+3 manikandan J wrote:
Dear Experts,

We have a Weld joint between Pipe to Hub as per sketch.

Run Pipe Thickness : 25.4 + 3 mm Cladding
Hub Thickness         : 31.8 + 3 mm Cladding    
Job Type : Weld joint in Piping
Code  : ASME B31.8-2020 Edn
image.png

Question 1 : For PWHT whether we need to consider Run pipe Thickness or Hub Thickness?.

Question 2 : If Run Pipe is considered for PWHT whether it includes Cladding Thk also?

Question 2 : If Hub is considered for PWHT whether it includes Cladding Thk also ?

Need your Views on this.

Regards,
Manikandan



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1c25eb99-b343-4309-ade0-0ae68b1bf506n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmM0X6z_F8ezxEnMCj4QejaocXqjE7b4rx_JLOFoDpsPxA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...