Re: [MW:33638] PTC Results vs Orientation of Impact Test Specimens

longitudinal  rolling direction will give better results.

On Wed, Oct 26, 2022, 8:59 AM williams p wilson <williamswilsonp@gmail.com> wrote:
Dear Experts,

Please advise, which orientation (Longitudinal or Transverse) impact tested plates will give the better PTC values later.Is there is any relation b/w PTC results and Orientation of Impact Test Specimens. This will guide me to select the suitable MTC for our project.

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ4JjPNs5v-z3k4VOqMaC_izaL9urCmX1%2BwsJ%3D3Mhiikhg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePc81wrDS822k5Oc%3Dj6AX0wdaxyK2FrJnDoda_napBRLg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...