Re: [MW:33631] welding Electrode for API 5CT L80 P110 Q125

Dear All,

Please suggest electrode for welding API 5CT pipe subject captioned Grades 
If any wps is available please provide 

Thanks & Regards
Hussain

On Tue, 25 Oct 2022, 8:51 am Hrushikesh Sangamnerkar, <hrushi612@gmail.com> wrote:
Thanks for the input.

Can you share the technical backup with the specific grade of SS..

On Fri, 21 Oct 2022, 14:51 'james gerald' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Use the below chart.

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Friday, 21 October, 2022 at 07:12:48 am GMT+4, Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:


Dear experts,

Query is can we weld Auto Tig (with Filler) for gas combination of Ar+Hydrogen? Pl provide technical literature to support the question,if available at your end.

Currently facing an issue of LOP with Argon gas only..

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2piyXRMx4A4tXavwmxnn-6dO4PkfAEZzw%2B4Cwd15h4TmA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/455856064.915055.1666343822485%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2oCY-KwiRKGUPomN6ascQLBus13KfPrK%3D1N55coqumFTQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKKjbk7Ny8515D4LW_oKii1XNGDm8acu7yTZ5S3K6aqLNZQJig%40mail.gmail.com.

No comments:

[MW:35693] egwuanimkwujacobisrael@gmail.com

Dear all, No. MPI can only detect defect that is 1 to 2 mm dept. Therefore the paint must have mask the defect. Thanks. Egwuanimkw...