Re: [MW:33626] Auto Tig for SS 310 with Ar+H2 gas

Hrishikesh we can use Ar 98% and 2%H2 with Filler wire. We use it for SigmaWeld Accelerated Tig, Square Butt Single Pass for SS310, with Filler.

Please connect will be able to help with some parameters...

We have used similar combination for capping passes as well. Tungsten angle will also play an important role

On Fri, 21 Oct 2022, 08:42 Hrushikesh Sangamnerkar, <hrushi612@gmail.com> wrote:
Dear experts,

Query is can we weld Auto Tig (with Filler) for gas combination of Ar+Hydrogen? Pl provide technical literature to support the question,if available at your end.

Currently facing an issue of LOP with Argon gas only..

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2piyXRMx4A4tXavwmxnn-6dO4PkfAEZzw%2B4Cwd15h4TmA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD%2BToCeh9E%2B875i6YKN2dHbRVaMy2VOT-_FOL0pAJCvFaiZPtw%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...