Dear Experts,

We have a Weld joint between Pipe to Hub as per sketch.

Run Pipe Thickness : 25.4 + 3 mm Cladding
Hub Thickness         : 31.8 + 3 mm Cladding    
Job Type : Weld joint in Piping
Code  : ASME B31.8-2020 Edn
image.png

Question 1 : For PWHT whether we need to consider Run pipe Thickness or Hub Thickness?. For set-in (Stub-in) connection, thickness of run Pipe and for set-on (Stub-on) connections, thickness of Header

Question 2 : If Run Pipe is considered for PWHT whether it includes Cladding Thk also? No

Question 2 : If Hub is considered for PWHT whether it includes Cladding Thk also ? No

Need your Views on this.

Regards,
Manikandan



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmORWERxzqJE4TfY58CzZxLA7J290D6Gqd1MV89zn%2BLVtA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...