Re: [MW:33608] Missing Material Certificate of Existing Line

You may go through the spectroscopic test for the existing pipeline. It may give you material compositions. Based on that composition you may find the material grade and yield.

On Fri, 21 Oct 2022, 11:36 am ilkinhasanov, <ilkinhasanov.91@gmail.com> wrote:
Dear All,

We have to weld our new fabricated pipeline to existing live line. (welding code is 1104).

Unfortunately,  we do not have a certificates of existing line. and it is not possible to perform shutdown to take a test coupons and perform chemical analysis and mechanical tests to identify grade of materials.

All knows that, existing line's material is Carbon steel but exact Yield and tensile Strength and Chemical prosperities are unknown. (our new fabricated pipeline is also Carbon steel.

Could you please advise me what can we do in this condition?



Regards,
Ilkin HASANOV

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d15ccca5-11f3-4b41-9fd5-7e88e8715ae8n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE%2B-gCazdMMi_a%3DnUeT-eFB88oVeNGNu3zr2jCeQSTe3QMKqmw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...