Re: [MW:33593] For preparing WPS on old PQR

hi sir, 
you can check the materials in the same group or not ?


Vào Th 5, 6 thg 10, 2022 vào lúc 12:14 Ritesh Kumar Singh <riteshsiwan770@gmail.com> đã viết:
Dear expert's,

I have pqr on material A516 GR.70 (SLEEVE) and A106 GR. B as per API 1104 APPENDIX -B. 
can I write a new WPS on the base of this PQR for material A537 CL.1 (SLEEVE) and API 5L X60.
 other parameters are same.

Regards
Ritesh kr. Singh.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-iM86uA0ApqoSsc21WBOUGmLoOgs4fpb9qReunQfRhvPA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-O%3DnS0E_TG_BMtnVa3ApTEYBF%3DTpYbFMepCgUuanqwEvnw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...