Re: [MW:33581] Internal Pressure Pipe Welding Hydro Test

Dear Sezgin,

                       There is an exemption for welded tubes & pipe internal under UW-2 (-a).

Thanks,

Kind Regards,

G.Gughan

On Tue, Oct 11, 2022 at 12:58 PM G Gughan <ggughan17@gmail.com> wrote:
Dear Sezgin,

                  Please refer to UW-2 (-a) for welded tubes & pipes internal. It is not considered under any category of UW-3. I hope it is correct & will assist you.

Thanks,

Kind Regards,

G.Gughan


On Mon, Oct 10, 2022 at 10:52 AM Sezgin Ckllı <euniversty@gmail.com> wrote:
Where can I find this explanation in Asme Sec.VII, can you explain this situation?

Thanks
10 Ekim 2022 Pazartesi tarihinde saat 06:25:35 UTC+3 itibarıyla Avanish Singh şunları yazdı:
For Internal Pipe , Don't Need to do Radiography.

On Sat, 8 Oct, 2022, 2:15 pm Sezgin Ckllı, <euniv...@gmail.com> wrote:
Hi ! 

The picture below shows the internal pressure inside the tank of the pipe. Does it need to be radiographically tested according to Asme Sec VIII Div.1?

Screenshot_1.jpg

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a698c2f0-0cb2-44cd-93f6-a15de0664398n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5ab4f7e3-a15e-437e-8f35-033e96e55de5n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB0bcTMCkHPtTZKtsMeCS4Jqm6bkJvZ56ixhS7-QP1zH1pMEdQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...