I too concerned about DSS cladding including DSS HEX tubes .
Is it ?
Vishwas
On Thursday, October 6, 2022 at 10:00:03 AM UTC+5:30 MW wrote:
Does the tube sheet have a lip? Please share a sketch at the weld location? practically it is difficult to avoid heat exposure to duplex clad? you need to change clad material, check with your process metallurgistOn Thu, 6 Oct 2022 at 09:52, Vishwas Keskar Welding Manager WELDING <vvkes...@gmail.com> wrote:Dear ExpertsOne of HEX involves following MOCs -HEX tubes - SA 789 TYP 32205Tubesheet -SA 266 CL 2 CS - Tube sheet IS cladded with TYP S32205 overlay.Shell side - CS -SA 516 GR 70 - 75mm thkChannel side - CS- SA 516 GR 70 - 75 mm thkPWHT is required for Tube sheet to Shell welding and Tube sheet to Channel welding. These are butt welds with CS Weld metal .PWHT is not required for Tube sheet to HEX Tube welding due to DSS tube to DSS cladding.Pl advice for the care that shall be taken during PWHT of Tube sheet to Shell welding and Tube sheet to Channel welding.Thanks and regardsVishwas - IWEInternational Welding Engineer
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/709cb8f5-63d1-437a-ba89-6b9c0ba7161bn%40googlegroups.com.
Comments