Re: [MW:33549] HEAT EXCHANGER CONSTRUCTION

Hi,
In general, DSS weld overlay is not recommended in CS due to cracking and other weldability issues. Moreover, Tube sheet forging with heavy weld overlay requires stress relieving too. 
However, stress relieving is not recommended for DSS, Hence in my opinion DSS weld overlay on TS to be replaced with Alloy 625 weld overlay wherein all these these issues related to weldability & PWHT will be solved.
Regards,
Prabhu.





From: Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com>
Sent: Thu, 06 Oct 2022 09:52:15
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:33541] HEAT EXCHANGER CONSTRUCTION

Dear Experts 
One of HEX involves  following MOCs -
HEX tubes - SA 789 TYP 32205 
Tubesheet -SA 266 CL 2 CS - Tube sheet IS cladded with TYP S32205  overlay.
Shell side - CS -SA 516 GR 70 - 75mm thk 
Channel side - CS- SA 516 GR 70 - 75 mm thk 
PWHT is required for  Tube sheet to Shell welding and Tube sheet to Channel welding. These are butt welds with CS Weld metal .
PWHT is not required for  Tube sheet to HEX Tube  welding due to DSS tube to DSS cladding.
 
Pl advice for the  care that shall be taken during PWHT  of Tube sheet to Shell welding and Tube sheet to Channel welding.
 
Thanks and regards
Vishwas - IWE
International Welding Engineer
 
 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a163c4a4-fe95-4245-bca0-099da2ddf579n@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1665030135.S.10013.29756.f5-224-128.1665063217.15589%40webmail.rediffmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...