Re: [MW:33542] HEAT EXCHANGER CONSTRUCTION

Does the tube sheet have a lip? Please share a sketch at the weld location? practically it is difficult to avoid heat exposure to duplex clad? you need to change clad material, check with your process metallurgist

On Thu, 6 Oct 2022 at 09:52, Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:
Dear Experts 
One of HEX involves  following MOCs -
HEX tubes - SA 789 TYP 32205 
Tubesheet -SA 266 CL 2 CS - Tube sheet IS cladded with TYP S32205  overlay.
Shell side - CS -SA 516 GR 70 - 75mm thk 
Channel side - CS- SA 516 GR 70 - 75 mm thk 
PWHT is required for  Tube sheet to Shell welding and Tube sheet to Channel welding. These are butt welds with CS Weld metal .
PWHT is not required for  Tube sheet to HEX Tube  welding due to DSS tube to DSS cladding.

Pl advice for the  care that shall be taken during PWHT  of Tube sheet to Shell welding and Tube sheet to Channel welding.

Thanks and regards
Vishwas - IWE
International Welding Engineer


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmTn8LwbHCudhjmWEG59GKo6WT01N-xmsRG4O1nB%3D3WSg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...