Dear expert
-- What is the filler wire for below mentioned mention Material
1. FILLER WIRE FOR HASTELLOY B TO HASTELLOY B BASE MATERIAL WELDING
2.FILLER WIRE FOR DUPLEX TO DUPLEX BASE MATERIAL WELDING
3. FILLER WIRE FOR ENCONEL 602 TO SS 316 BASE MATERIAL WELDING
Best regards
Sujit kumar