[MW:33621] PTC Results vs Orientation of Impact Test Specimens

Dear Experts,

Please advise, which orientation (Longitudinal or Transverse) impact tested plates will give the better PTC values later.Is there is any relation b/w PTC results and Orientation of Impact Test Specimens. This will guide me to select the suitable MTC for our project.

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ4JjPNs5v-z3k4VOqMaC_izaL9urCmX1%2BwsJ%3D3Mhiikhg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS