i have query , We can do RT for weld Joint with painting , Its allowed , In our site they did RT with painted joint with out client approval
They will be problem that may hide weld defect , painting DFT 300 to 400 micron
If allowed do RT with Painting , Please share some supporting documents
Thanks for your support
Best regards
Sankar.k
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ac980cb1-6c30-40ef-8a12-5c5cbcc44700n%40googlegroups.com.
Comments