Base metal between 5 and 30 mm
My design temperature : -46
Impact Test : -46°C 27J
PWHT : 620°C
The materials are SA516 Gr60 and SA516 Gr70.
I want to do a PQR test for the first time but I don't know where to start and how to research.
For example, how many mm thick material, how many mm GTAW and how many mm SAW weld should I use for my PQR to work properly.
-- My design temperature : -46
Impact Test : -46°C 27J
PWHT : 620°C
The materials are SA516 Gr60 and SA516 Gr70.
I want to do a PQR test for the first time but I don't know where to start and how to research.
For example, how many mm thick material, how many mm GTAW and how many mm SAW weld should I use for my PQR to work properly.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0410faa8-5a30-49f4-a8c2-46989e0b1a29n%40googlegroups.com.
Comments