Re: [MW:31388] E-7018-1 is better then E7018

When subjected to SR, 7018-1 gives better mechanical value compared to 7018 due to more manganese in -1. Better ductility , cost is more

On Wed, 2 Sep 2020 9:19 pm HENNING John, <John.Henning@hamon.com> wrote:

Consider it to be a premium subset of the E7018.  Basically same properties but with chemistry optimized to achieve low temperature impact properties.  It is generally acceptable to use E7018-1 in lieu of E7018 unless customer has specific requirements regarding qualification. 

 

Code is fun. Enjoy.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of George Dilintas
Sent: Wednesday, September 02, 2020 7:13 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:31385] E-7018-1 is better then E7018

 

Better performance in low temperature. Same A and F-no

 

Στις Τετ, 2 Σεπ 2020 στις 9:00 π.μ., ο/η Ghulam Mustafa <gmt.lah@gmail.com> έγραψε:

Dear All,

Hope you are fine.

i want discuss that i was gone yesterday for inspection in other company as a third party, i checked WPS for welding inspection, during inspection i observed that welder used E7018-1 Electrode instead of E7018 on structure. structure material A572 Grade-B and A-36. E7018-1 can problem or not?

can any one tell me about this problem.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b55e87f5-633e-477c-b7ad-be9aa33fcd52n%40googlegroups.com.


 

--

Dr. Georgios Dilintas,

Dipl. Ing. In Aeronautic and Space Engineering

Ph.D in Mechanics of Solids - Computational Mechanics

A.I.S, A.N.I, IRCA Lead Auditor

Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40BPcbycTuOvuJCNEMB8qdtqAO02sgof5q6ZVzqHKbwMeQ%40mail.gmail.com.

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/AM7PR01MB70768193C0A7E65862DA17C2902F0%40AM7PR01MB7076.eurprd01.prod.exchangelabs.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOQ3gSG%3Dqe4DuhGD8VKpHaPPGvO5d2rjXZPc-OW9awsPw%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...