Thursday, September 3, 2020

[MW:31387] RE: 31380] E-7018-1 is better then E7018

Hi Ghulam,

E 7018-1  electrodes contains more Mn than E-7018 electrode, at the same strength(UTS) level, 70 Ksi. The advantage is better impact . Typically E-7018-1 are designed for impact up to -46 Deg c , while the same for E-7018 is up to -29 Deg C.

In order to avoid duplicity or redundant work nowadays  it's very commons for electrode manufacturers to classify same welding electrode as E-7018-1/E-7018, which is called dual certification.

Please look at the highlighted text from, SFA 5.1 , Sec-II, Pt-C, on E-7018-1 welding electrodes.

As the mechanical and other properties of the deposited are not changed, a change from E-7018 to E-7018-1 , will not cause any harm the welds . However if should be addressed in WPS or regularized through an NCR.

 

Thanks

 

Pradip Goswami, P.Eng, IWE

Consultant-Welding-Metallurgical Engineering

 

Cell & Whatsapp-905-9793232.

Personal:pgoswami@rogers.com

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Ghulam Mustafa
Sent: September 2, 2020 1:06 AM
To: Materials & Welding <
materials-welding@googlegroups.com>
Subject: [MW:31380] E-7018-1 is better then E7018

 

Dear All,

Hope you are fine.

i want discuss that i was gone yesterday for inspection in other company as a third party, i checked WPS for welding inspection, during inspection i observed that welder used E7018-1 Electrode instead of E7018 on structure. structure material A572 Grade-B and A-36. E7018-1 can problem or not?

can any one tell me about this problem.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b55e87f5-633e-477c-b7ad-be9aa33fcd52n%40googlegroups.com.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...