Skip to main content

Re: [MW:29998] Boiler without S Stamp delivered to site

Dear ,

Please find the reply 
  1. Hydrotest requirement (Shop or Site) ITP/PCP .?? Hydrotest carried at Shop as per ITP and project requirement to do at site . And contractor will perform site hydro test .
  2. In MDR hydrotest pressure or position mentioned.?? Hydro pressure Mentioned .
  3. Hydrotest Date in Name Plate .??  .dates not mentioned.
  4. Is it NBIC registered equipment .?? NBIC Registered.  
Any further suggestion , advise why it was not stamped @ shop.

Thanks and Regards
Abraham


On Mon, Aug 26, 2019 at 1:23 PM Dhanabal Jalachandran <dhanabal.jalachandrann@gmail.com> wrote:
Dear Friend,

Name Plate and MDR are two very important documents while manufacturing any equipment with ASME requirements.

Verify the below points before taking any decision,
  1. Hydrotest requirement (Shop or Site) ITP/PCP .??
  2. In MDR hydrotest pressure or position mentioned.??
  3. Hydrotest Date in Name Plate .??
  4. Is it NBIC registered equipment .??
Br
Dhanabal Jalachandran

On Sun, Aug 25, 2019 at 2:03 PM Abraham Abi <a.p.abraham2010@gmail.com> wrote:
Dear experts 

 In our project we received Utility Boiler without S Stamp in Name Plate . Contractor response is hydro test will be done with AI involvement and final stamping will be done .
 
 But manufacturer supplied MDR documents signed by AI , certified with S stamp mentioning shop hydro test , thk , dimension details all.

 My query , if MDR is stating S stamp , why it was not stamped in Name plate at shop and delivered to site.
 
Thanks & Regards
Abraham 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOsuTKndp4%2BW0N%2BtsNJ2cOzdsGswgGJiHLd3wdX0GKWtmEQrZg%40mail.gmail.com.


--
Regards
Dhanabal Jalachandran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPLwtDd-tt2x8ZAR6WdGggPCCouyVWLvVP3J8OetH5LfMH6JWw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOsuTKkb_RnMR_-J34yietsEL_f-DgsqkxhN7mYUUUW1BT9jZQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...