Re: [MW:29912] Impact testing as per ASME B31.3

You may please refer to Table 323.3.1 Impact Testing Requirements for Metals of ASME B31.3, Chapter 3.


Below is the snapshot, Refer A.5 


 



Regards,

Sudhakar K

Welding Engineer



On Thu, Aug 1, 2019 at 8:19 AM pradip kumar Sil <pradipsil@gmail.com> wrote:
Can you pls give reference for qualification thickness in this case



On Wed, 31 Jul 2019, 09:25 Sudhakar Kuppuswamy, <mechsudhakar@gmail.com> wrote:

In my opinion, for the below stated conditions, as per ASME B31.3, Impact test is applicable. I.e. supplementary essential variables for ASME Section 09 becomes essential variables. 

And, the qualified WPS thickness shall be T/2 to T+6mm, i.e. 8.74 mm to 23.48 mm in your case.


Regards,

Sudhakar K

Welding Engineer 




On Wed, Jul 31, 2019 at 11:24 AM Babur Khan <mbabur.bwp@gmail.com> wrote:
Dear experts, 
Please clarify for impact test requirements of below variables.
Construction code ASME B31.3
Material A106 Gr. B
The thickness of Pipe. 17.48 mm
Temperature Limit 0^ F (-17.78^ C)
PWHT yes.
Table A-1 refers to curve B
Table 323.2.2A minimum Temperature without Impact Testing for CS showing under curve B 9^ F ( 12.8^ C).
My Question is for above case Impact testing for WPS qualification is required?  

Regards,

Muhammad Babur Khan Lashari
Sr. QA/QC Inspector (Welding)

(CSWIP 3.1 / CWI II From PWI) 

Mob: + 966 58 2774568 / 050 5193275

PAK : + 92 334 6186285 (Whatsapp)

Skype: babur.lashari

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN53wK1Vs8CgXP0uzAFyPAUNQ-gbaeg7axU9zRQZsXhV9p19jg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BfZfcPjTGp6RdR8Q_-4Q%2B_AxS3cG4_scXWH2m-b3fW-5apgzg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8ko-s%3DXUi90qaiSkw43p_dXnuWxb7k1oom%3DhxNtfFkhRQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BfZfcP0-RffjshZenc%2BQOKMtknKLVJ7Owz4k6WW%2BPP-zb7OEA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...