Hello Sangram ,

A) Exactly As per code your welder only qualify for Gtaw process   , then how he can weld use for SMAW process.

And In B condition he can not weld below 75 mm od size pipe.

Regards ,
Sumit Bhadakwad

On Tue, 6 Aug 2019 at 19:04, 'Sangram' via Materials & Welding <materials-welding@googlegroups.com> wrote:
 Mr. Swaminathan
Actual joint size 2inch & 19mm  thickness 

Regards 
Sangram 

Sent from my iPhone

On 06-Aug-2019, at 7:25 AM, Kishor Swaminathan <kishors28@gmail.com> wrote:

Dear 

Sangram' via Materials & Welding


yes we can , how much the actual thickness 

Regards,
KISHOR SWAMINATHAN
WELDING INSPECTOR 


On Tue, Aug 6, 2019 at 7:03 AM 'Sangram' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear experts
Please give me your valuable feedback with code reference.
A) One welder is qualified with dia 1" & above with GTAW(11mm)
B) Same welder also qualified with 2 7/8 & above with GTAW + SMAW (7.5 mm Gtaw + max to be welded smaw )
My question:
Can this welder welded any 2" joint which thickness is more than 11mm by using GTAW+SMAW process ??

Regards
Sangram

Sent from my iPhone

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/E4DEF482-CEE0-4A77-A796-AA166751B51E%40yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPd%2B2RSxmR%3DMPk6G2upA8fqu56v7X04uSDgXBv39KhysWe4LMA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CC923824-84FE-41FA-AE3A-16AF2EB18271%40yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKkx5R1ZhN%3DoFMr0jmg%3DUVvsbQL8OGhHixWUgt-Qb%3D5j%2B2vtBQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...