He leak test will detect through and through discontinuities. PT will detect open to surface discontinuities. Hence Surface discontinuities will not be revealed by He leak test.
P. V. Ghanekar 

On Sun, 29 Apr 2018 08:55 chiluka venkatramulu, <ramuluchiluka@gmail.com> wrote:
Helium leak test is more effective than PT test. It will detect minute leaks. Its sensitivity also high. In my opinion it can be accepted.Before that you need to accept their procedure and leak rate.

Venkatramulu

On Sat, Apr 28, 2018 at 4:32 PM, Makrand Sakpal <makrands9@gmail.com> wrote:

Dears, 


For tube-to-tubesheet joints in air cooled heat exchangers, can helium leak test be a substitute for PT test? One of our vendor have proposed helium leak test in lieu of PT test for tube-to-tubesheet joints.


Vendor have provided following justification,

We have offered a helium leak test after welding the tubes, in lieu of the requested liquid dye penetrant testing of the T/TS welds. We have found that the application process of spraying the liquid penetrant and developer through a plug hole using an aerosol can is ineffective as it is difficult to control the amount of chemicals being applied. we have even experienced on some jobs where excessive penetrant of developer solidifies giving false negative/positive results causing unnecessary rework or obscuring potential indications (leaks). if PT testing is desired over the helium leak testing, we can perform the testing at no charge, but will not guarantee or provide a report stating the results were acceptable. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...