Re: [MW:27742] Dia range.for WPS as per API 1104

Hi

API 1104 covers welding procedures qualifications as below,

Case

1.    Clause 5 Welds Containing Filler-metal Additives

2.    Clause 12 Mechanized Welding with Filler Metal Additions

3.    Clause 13 Automatic Welding Without Filler metal Additions

 

 

Diameter range is not essential for case 1 WPS/PQR, i.e. 5.3.2.3 however "the ranges of outside diameters and wall thicknesses over which the procedure is applicable shall be identified".

 

Means unlike ASME sec 9, WPS/PQR format, additionally you may need to specify the restriction on outside diameter and thickness in order to facilitate to have control on welders use in production welding ( based on clause 6.2.2 d )


Diameter range for case 2 & 3 WPS/PQR is essential variable, refer respective clauses - 12.5.2.5 & 13.5.2

 

 

Also refer API 1104 interpretation ( specifically Page 82 /94 ) attached herewith for more details. There are many questions based on this topic only.

 

Downloaded from

http://mycommittees.api.org/standards/techinterp/transpipe/default.aspx

 

 






On Sun, Apr 22, 2018 at 10:04 AM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Non essential. There is no limit on pipe dia. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sun, Apr 22, 2018 at 9:40 AM, CEIL Mumbai <bpplceil@gmail.com> wrote:
6.2.2(d)is for war not for wps

On Sun 22 Apr, 2018 8:17 am 'ramen samanta' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear Joydev

Pl. ref. API- 1104- clause 6.2.2 (d)- dia. groups

Thanks,

R.K.Samanta



On Saturday, 21 April, 2018, 11:57:31 AM IST, joydev dalai <joykolkata07@gmail.com> wrote:


Dear Expert,

Please suggest Dia range.for WPS as per API 1104.

--



Best Regards,

Joydev Dalai
Dy. Manager - QA/QC
+91-6202987794
Kalpataru Power Transmission ltd.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...