Re: [MW:27724] Distance between two L-Seam

WHY DISTANCE REQUIRED??

KRUNAL

On Thursday, March 28, 2013 at 4:47:35 PM UTC+5:30, Gurunath Hanamar wrote:
Dear Mr. Himanshu,

As per B 31.3 seam to seam minimum distance is given as 4 times thickness but B 31.3  haven't mentioned L seam to L seam staggering. Means can be weld without staggering.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards, 
Gurunath Hanamar


On Thu, Mar 28, 2013 at 11:11 AM, Himanshu Patel <absg...@gmail.com> wrote:
Hello To ALL,
 
This clause applicable to Pressure Vessel, What about PIPING can any one suggest for piping as per (API 1104, B31.4, B31.3 or B31.1).
 
Thanks.
 

On Thursday, June 14, 2012 11:56:49 AM UTC+4, saravanan sornam wrote:
Hi Guru,
 
You can find in ASME VIII Div. I, UW-9 (d).
 
(d) Except when the longitudinal joints are radiographed
4 in. (100 mm) each side of each circumferential welded
intersection, vessels made up of two or more courses shall
have the centers of the welded longitudinal joints of adjacent
courses staggered or separated by a distance of at
least five times the thickness of the thicker plate.
 
Hope it is Ok for U...
 
Cheers,
Sarav,
Korea

On Thu, Jun 14, 2012 at 12:24 PM, Gurunath.Hanamar <guru...@gmail.com> wrote:

Dear all,
I know that 100mm is permissble distance between two consecutive longitudinal seams but, can any one confirm minimum distance between two longitudinal seams should be mantained. Kindly mention ASME clause.

Thanks &Regards
Gurunath Hanamar

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...