Tuesday, April 17, 2018

Re: [MW:27716] Stellite 6 hard facing by GMAW process

Hi Prasad,

stress revealing cracks will be there .but dont worry ,Its the property of the material ( low  ductility). please use Ni based base layer ,on top deposit  ST-6.

Kr
shyamal


On 17 April 2018 at 10:05, N VENKATESWARA PRASAD <weldengr.velosi@gmail.com> wrote:
Dear Experts,

Please share your experience stellite 6 hard facing by GMAW ( CMT/ STT ) process to achieve crack free deposit.

Regards

Prasad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...