Wednesday, April 11, 2018

Re: [MW:27695] Re: WPS base metal qualification range

Two materials are mentioned in the original mail P5A and below in that mail mention P15E, I guess there is a confusion here, specifically I refer to the material P5A, THAT WAS THE POINT THAT I EXPOSE.
Please see attached image.



Hi 

This is Srinivas, 

I got a PQR P5A to P5A , So i can write WPS P5A to P4 from that P5A to P5A PQR ? 

Based on QW 424.1 ? 

On Sunday, 6 April 2014 12:18:17 UTC+8, Binoy Lonappan wrote:
As per Section IX QW 424 for procedure qualification it is given thatt 

for base material range of qualification as P15 E metal to P4 metal is 
qualified for any metal from P15E to P4 or P3,P1 
But P number is an essential variable so what is the actual 
interpretation of the above clause 

Or does it means if we qualify procedure for P15E +P4 then it is 
qualified for the P15E any metal from this group to any metal from 
P4,P3 P1 groups



2018-04-11 9:04 GMT-05:00 George Dilintas <dilintas@gmail.com>:
You have to read QW 403.1 and then QW 424 carefully. Your interpretation is wrong . If your PQR was done using a P15E and a P4, then you can support WPS which are for any P15E to any P4 ONLY

2018-03-28 10:38 GMT+03:00 srinivas <srinivasduraisamy@gmail.com>:
Hi 

This is Srinivas, 

I got a PQR P5A to P5A , So i can write WPS P5A to P4 from that P5A to P5A PQR ? 

Based on QW 424.1 ? 

On Sunday, 6 April 2014 12:18:17 UTC+8, Binoy Lonappan wrote:
As per Section IX QW 424 for procedure qualification it is given thatt

for base material range of qualification as P15 E metal to P4 metal is
qualified for any metal from P15E to P4 or P3,P1
But P number is an essential variable so what is the actual
interpretation of the above clause

Or does it means if we qualify procedure for P15E +P4 then it is
qualified for the P15E any metal from this group to any metal from
P4,P3 P1 groups

--
With Regards
Binoy Lonappan
+91-9645100560
QAC Engineer
TECCL

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Ing. José Juan Jiménez Alejandro

ASME Independent Consultant 

and Technical Manager SSI-TPI

Cel. +52 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...