Wednesday, April 11, 2018

Re: [MW:27686] ASTM A572 Gr50 TMCP

572 is not come under TMCP??

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Wed, Apr 11, 2018 at 4:47 PM, nguyen tuan <tuanpvecc@gmail.com> wrote:

Dear Expert,

We have bought a plate ASTM A572 Gr. 50 with condition supply: TMCP
Our Client asking that when are acceptable for TMCP for ASTM A572 gr. 50

Could you pls. help us reply the question.

Thank best regards,

Nguyen Anh Tuan

QC inspector

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...