The 2016 edition of B31.1 is requiring VOLUMETRIC EXANIMATION (RT or UT).
it is surprising that this Code Section has no lower thickness limit for UT. However Section I does not allow UT when the thickness is lower than 13 mm (see Table PW-11 note f). 

2018-04-04 6:39 GMT+03:00 <email2ragkiran@gmail.com>:
Dear Pradip,
Yes, you can perform UT in lieu of RT, refer to code cases B31 - case184 and 2235-9. Deviation request can cover this requirement.

Regards,
Kiran

On Wednesday, March 7, 2018 at 5:52:01 AM UTC+3, pradipsil wrote:
Dear Everybody,
Can we perform  UT on the pipe joints as per ASME Sec 1 or B31.1 instead of RT.
Pls clarify with code references.
Thanks in advance
Regards
Pradip

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...