Wednesday, April 11, 2018

Re: [MW:27679] Percentage of RT As Per ASME B31.3

start reading 341.4
for normal fluid services, RT is 5%.
For severe cyclic conditions, it is 100%
For elevated temperature service there is a requirement for the NDE during the fabrication of the pipes in the mill. 100% RT on longitudinal or spiral welds if base metal is Pno 4 or 5

2018-04-11 13:48 GMT+03:00 Mukul <mukulhossen70@gmail.com>:
Dear Experts,

Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?




Regards,

Mukul Samad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...