Hello prasad,
No need to do ferrite testing for SA 312 TP 316 L Welding, because this all are austenitic stainless steels. 
  Ferrite testing is applicable for Duplex stainless steel because it is a ferritic steels. 
For SA 312 TP 316 L Welding procedure you have to do IGC practice E or it may as per client requirements.
If any thing wrong,  I am apologies for the same. 
Regards, 
  Rajendra 
On 8 Apr 2018 6:41 p.m., "Prasad Rode" <purode333@gmail.com> wrote:
Dear sir,--
I am going to do PQR for SA 312 TP 316L pipe to pipe of 6" and 7.11mm thickness.
I want to know that, i have to go for ferrite testing or not ?
If not, when it is essential to ferrite testing?
Regards
Prasad
https://materials-welding.blogspot.com/ 
https://www.linkedin.com/groups/122787 
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments