Friday, April 28, 2017

Re: [MW:26488] DIN Wire IQI Thickness

10ISO16 WIRE
API-1104 JOB THK 11.1
API1104



PATEL KUNJAL  
INSPECTION ENGINEERSGS INDIA PVT LTD
M: 9549977588 




On Fri, Apr 28, 2017 at 11:48 AM, PATEL <kunjpatel1991@gmail.com> wrote:
Dear sir
DIN ISO 10ISO16 WIRE JOB THK 11.1 CAP+2MM RT FILM NUMBER OF IQI SHOW 

On Monday, May 31, 2010 at 8:25:02 AM UTC+5:30, manpreet singh wrote:
Hi
Refer ASTM E747 for IQI radiography.

Regards
Manpreet Singh
Welding Engineer
Spiecapag

On Sun, 30 May 2010 14:10:38 +0530 wrote
>Dear All



Where to we find DIN wire IQI Thickness?

Which standard is deals about DIN wire IQI Thickness?

Where to refer?



--

To post to this group, send email to material...@googlegroups.com

To unsubscribe from this group, send email to materials-weld...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/I36HrxlDnSQ/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/51666b0a-b280-4481-800a-e5b846e5f5df%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANAk%3DpyvyqVoqz28-r8ABMbuFB%3DPOCwRnnrq8BV2m_QFRJ_juw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...