Dear Anil,

You change the orientation or rotate the LSAW pipe (main pipe) if possible.

Otherwise get clarification or approval from your design engineering.

Once approved you can do
Welding.

Please note that after welding of branch pipe (with or without RF Pad), additional radiography of 150 mm (both sides) shall be taken on main pipe long seam weld to ensure the weld metal soundness.

The above radiography requirement is  more enough to satisfy the Client.

Regards
P Govindan

On Mar 17, 2013 12:51, "Anil Hegde" <nottyanil@gmail.com> wrote:
Dear Expert ,

We have a 36 inch pipe which is welded type ,On it We have 12 inch connection which is coming on the ( long seam ) of the pipe .

Is There any code which says we can or cannot do welding on long seam of the pipe .

Requesting you for your positive feedback .

Regards
Anil Hegde 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9fJHM-ss5J%3Dzfcu2kofLsZW4ZEnubDb--JHxFcxjtqNEw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...